特性級別 | 標準級|||高流動|||高圄沖||| |
牌號 | GH42 |
加工級別 | 注墮級||| |
品名 | PP HANWHA TOTAL Hanwha GH42 |
廠家(產地) | 韓國三星TOTAL/韓華 |
用途級別 | 汽車部件|||電子電器部件|||家電部件||| |
PP 三星 GH42 價格
PP GH42 HANWHA TOTAL Hanwha
Hanwha Total PP GH42
高結晶性聚丙烯
玻璃纖維增強材料
HANWHA TOTAL PETROCHEMICALS Co., Ltd.
產品說明:
GH42 is a G/F modified polypropylene compound modified by glass fiber filling to improve mechanical rigidity and heat-resistance. It is produced by modifying a variety of base PPs, including HIPP (High Isotactic Polypropylene), with Hanwha's special processing technology. Its excellent quality makes it ideal for use in air conditioner fans and automobile cooling fans; and like products requiring high rigidity and high impact-resistance.
填料/增強材料 |
|
特性 | 尺寸穩定性良好低翹曲性剛性,高高拉伸強度高強度間苯二甲抗撞擊性,高可加工性,良好流動性高耐熱性,高阻燃性 |
用途 | 電氣/電子應用領域電氣元件電器用具動力/其它工具工業應用混合家用貨品汽車領域的應用 |
形式 |
|
加工方法 |
|
PP 三星 GH42 價格
PP GH42 HANWHA TOTAL Hanwha
物理性能 | 額定值 | 單位制 | 測試方法 |
比重 | 1.04 | g/cm3 | ASTM D792 |
熔流率(熔體流動速率) (230°C/2.16 kg) | 10 | g/10 min | ASTM D1238 |
收縮率 - 流動 (2.00 mm) | 0.30 到 1.0 | % | ASTM D955 |
硬度 | 額定值 | 單位制 | 測試方法 |
洛氏硬度 (R 級) | 114 | ASTM D785 |
機械性能 | 額定值 | 單位制 | 測試方法 |
抗張強度 3 | 88.3 | MPa | ASTM D638 |
伸長率 3 (斷裂) | 4.0 | % | ASTM D638 |
明顯的彎曲模量 | 108 | MPa | ASTM D747 |
彎曲模量 4 | 4120 | MPa | ASTM D790 |
沖擊性能 | 額定值 | 單位制 | 測試方法 |
懸壁梁缺口沖擊強度 (23°C) | 98 | J/m | ASTM D256 |
熱性能 | 額定值 | 單位制 | 測試方法 |
載荷下熱變形溫度 (0.45 MPa, 未退火) | 162 | °C | ASTM D648 |
可燃性 | 額定值 | 測試方法 | |
UL 阻燃等級 | HB | UL 94 |
注射 | 額定值 | 單位制 | |
料筒后部溫度 | 180 到 220 | °C | |
料筒中部溫度 | 180 到 220 | °C | |
料筒前部溫度 | 180 到 220 | °C | |
模具溫度 | 50.0 到 80.0 | °C | |
注塑壓力 | 49.0 到 88.3 | MPa | |
背壓 | 0.490 到 0.981 | MPa | |
螺桿轉速 | 30 到 80 | rpm | |
注射說明 | |||
Injection Speed: max |
PP 三星 GH42 價格
PP GH42 HANWHA TOTAL Hanwha